Polymer Property : Vicat Softening Point = 383 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point >= 195 °C

@Load 5.001 kg
>= 383 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANAMID 66.6 C22^E F Nylon 66/6, Modified
Information provided by Polykemi AB
Vicat Softening Point >= 195 °C

@Load 5.001 kg
>= 383 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B/C12^ F30 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Vicat Softening Point 195 °C
383 °F
ISO 306
Radici Radilon® S35HR (dry) Nylon 6
Medium high viscosityInformation provided by Radici group.
Vicat Softening Point 195 °C
383 °F
B
Plastcom SLOVAMID 6 GF 5 PA6, 5% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 5% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Vicat Softening Point 195 °C
383 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Vicat Softening Point 195 °C

@Load 5.00 kg
383 °F

@Load 11.0 lb
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Vicat Softening Point 195 °C

@Load 5.00 kg
383 °F

@Load 11.0 lb
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Vicat Softening Point 195 °C

@Load 5.00 kg
383 °F

@Load 11.0 lb
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi..
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for..
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East)
NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability.
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East)
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East)
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 6
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 195 °C
383 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 195 °C
383 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL HH180 PPE+PS
Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365.
Vicat Softening Point 195 °C
383 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East)
Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365.
Vicat Softening Point 195 °C
383 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 195 °C
383 °F
50°C/h 50N; ISO 306
DSM Akulon® K222-D (Dry) Low Viscosity Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Vicat Softening Point 195 °C
383 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Vicat Softening Point 195 °C
383 °F
50°C/hr; 50N
Arkema Group Orgalloy® RS 6630 Nylon 66 Alloy, 30% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..