Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 414 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
Melting Point 212 - 224 °C
414 - 435 °F
Average value: 216 °C Grade Count:29
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Lanxess Durethan® C 38 FA 000000 Copolyamide
Copolyamide, film quality, high transparency, with slip agent, not nucleatedApplication Examples: blown film coextrusion (central layer)
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Lanxess Durethan® C 38 FKS 000000 Copolyamide
Copolyamide, film quality, high transparency, with processing aid, nucleatedApplication Examples: blown film coextrusion (outer layer)
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® C 38 FAM 000000 Copolyamide
PA 6-Copolymer, non-reinforced, extrusionInformation provided by LANXESS.
Melting Point 212 °C
414 °F
Solvay Technyl® C216V30 30% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Melting Point 212 °C
414 °F
DSC
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Melting Point 212 °C
414 °F
By DSC
Toyobo PELPRENE™ P150B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Melting Point 212 °C
414 °F
By DSC
Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
Melting Point 212 °C
414 °F
ISO 3146
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EM630 63 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EM631 TPC-ET
Extrusion Grade
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PL381-H TPC-ET
Injection Molding
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET  (Unverified Data**)
Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent ..
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Melting Point 212 °C
414 °F
ISO 3146
Cathay PA511 Renewable Engineering Polyamide
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr..
Melting Point 212 °C
414 °F
ASTM D3418
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced
A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
Melting Point 212 °C
414 °F
ASTM D3418
Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced
A 40% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
Melting Point 212 °C
414 °F
ASTM D3418
Ashley Polymers Ashlene® 980LS-43GB Nylon 612, 43% Glass Reinforced
A 43% glass reinforced, heat stabilized Nylon 612 resin in black.Data provided by the manufacturer
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 212 °C
414 °F
DSC
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Copyright © lookpolymers.com All Rights Reserved