Polymer Property : UL RTI, Mechanical with Impact = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC
Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 3101-20 Polyester BMC
Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 104 PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific)
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not ..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 141R PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 201 PC
7.0 MFR, for thicker sections without sinks. Improved flame retardance.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific)
7.0 MFR, for thicker sections without sinks. Improved flame retardance.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific)
10.5 MFR. Improved flame retardance. Internal mold release.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HF1140R PC
High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® ML7678 PC
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific)
LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HP4 PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL temperature Index, UL 746B
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL temperature Index, UL 746B
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL temperature Index, UL 746B
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific)
Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release.