| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Decomposition Temperature | 375 °C | 707 °F | 1% Mass Loss, Air |
|
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers.
|
|||
| Decomposition Temperature | >= 375 °C | >= 707 °F | @ 1% weight loss; TGA |
|
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
|
|||
| Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
|
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt. loss / in air |
|
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt. loss / in air |
|
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt. loss / in air |
|
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | ASTM E1131 |
|
Zeus PVDF Tubing
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | Degradation Temperature |
|
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
|
|||
| Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
|
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
|
|||
| Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
|
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt. loss / in air |
|
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 375 °C | 707 °F | 1% wt loss / in air; TGA |
|
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||