| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Decomposition Temperature | 410 °C | 770 °F | 1% Mass Loss, N2 |
|
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers.
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt. loss / in nitrogen |
|
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt. loss / in nitrogen |
|
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt. loss / in nitrogen |
|
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt. loss / in nitrogen |
|
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Decomposition Temperature | 410 °C | 770 °F | 1% wt loss / in nitrogen; TGA |
|
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||