Polymer Property : Maximum Service Temperature, Inert = 151 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 151 °C
304 °F
Heat Deflection, load unknown
Malvern Minerals Diallylphthalate with Methallylate Silane Treated Novakup® 1250 Quartz Filler
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 1.0% Z-6030 methallylate silane) filler. Separate entries demonstrate the effect of untreated NovaciteÂ..
Maximum Service Temperature, Inert 151 °C
304 °F
Heat Deflection, load unknown
Malvern Minerals Diallylphthalate with Vinyl Silane Treated Novakup® 1250 Quartz Filler
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 1.0% Z-6075 vinyl silane) filler. Separate entries demonstrate the effect of untreated Novacite® fil..