Processing Temperature | 135 - 180 °C | 275 - 356 °F | Average value: 162 °C Grade Count:22 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic.. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 3 hr. |
Von Roll Isola IMI Varnish 3255 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 3 hr. |
Von Roll Isola IMI Varnish 73523 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 6-18 hr. May also be cured for shorter time at higher temperatures. |
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 180 °C | 275 - 356 °F | Average value: 162 °C Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 135 - 293 °C | 275 - 560 °F | Average value: 263 °C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |