| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 210 - 250 °C | 410 - 482 °F | Barrel Temperature |
|
SABIC PP 511A Polypropylene Homopolymer for Spunbond Applications
Product Description: PP 511A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 511A has the following features:Consis..
|
|||
| Processing Temperature | 210 - 235 °C | 410 - 455 °F | Barrel Temperature |
|
SABIC PP 578P Polypropylene Homopolymer for Injection Molding
Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr..
|
|||
| Processing Temperature | 210 - 250 °C | 410 - 482 °F | Injection molding cylinder temperature |
|
LG Chemical HI835S PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||
| Processing Temperature | 210 - 250 °C | 410 - 482 °F | Injection molding cylinder temperature |
|
LG Chemical HI855S PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||
| Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
|
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Processing Temperature | 210 - 260 °C | 410 - 500 °F | |
|
IRPC Polimaxx Polene 120PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
|
|||
| Processing Temperature | 210 - 260 °C | 410 - 500 °F | |
|
IRPC Polimaxx Polene 320PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
|
|||
| Processing Temperature | 210 - 260 °C | 410 - 500 °F | |
|
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
|
|||
| Processing Temperature | 210 - 240 °C | 410 - 464 °F | injection |
|
IRPC Polimaxx Polene GP110 Polystyrene
APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc.
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
|
IRPC Polimaxx Polene GP150 Polystyrene
APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc.
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
|
IRPC Polimaxx Polene HI650 Polystyrene
APPLICATIONS: INJECTION MOULDING, ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARES. etc.
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 210 °C | 410 °F | |
|
Shinil Chemical SHINNANO PP Polymer Nanocomposite Bumper
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
|
|||
| Processing Temperature | 210 °C | 410 °F | Transition Temperature |
|
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Processing Temperature | 210 °C | 410 °F | Transition Temperature |
|
SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | C2 |
|
UBE 1022FDX23 Nylon 6 Homopolymer Film
Specialties: High slip typeProcessing: Water cooling processTypical applications: small pouch & generalInformation provided by UBE.
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | C2 |
|
UBE 1024FDX41 Nylon 6 BOPA Film
Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE.
|
|||
| Processing Temperature | 210 - 220 °C | 410 - 428 °F | C3 |
|
UBE 7034B Nylon 6/12 Copolymer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
|
|||
| Processing Temperature | 210 - 260 °C | 410 - 500 °F | |
|
E-Polymers Tekaloy® G70FR , Flame Retardant, Un-Reinforced PC/ABS Alloy
Flame Retardant, Impact ResistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f..
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Range |
|
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Range |
|
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Processing Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion Range |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Processing Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion Range |
|
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Range |
|
Arkema Group Pebax® MX 1205 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MX 1205 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to mee..
|
|||
| Processing Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Range |
|
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Processing Temperature | 210 °C | 410 °F | Gate Temperature; Extrusion |
|
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Processing Temperature | 210 - 220 °C | 410 - 428 °F | Injection |
|
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer
Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Processing Temperature | 210 - 250 °C | 410 - 482 °F | Injection molding cylinder temperature |
|
LG Chemical HI835H PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||
| Processing Temperature | 210 - 250 °C | 410 - 482 °F | Injection molding cylinder temperature |
|
LG Chemical HI835M PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||