| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes
BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BB108E Polypropylene compound for Steel Pipe Coating
BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating
Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio..
|
|||
| Head Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis BorECO™ BEC5015 Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BEC5015 is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength.BorECO BEC5015 is recommended for solid wall and structured wall n..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-1498 Polypropylene Random Copolymer
RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-2491 Polypropylene Random Copolymer
RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-6015 Polypropylene Random Copolymer
RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-6017 Polypropylene Random Copolymer
RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-2492 Polypropylene Random Copolymer
RA130E-2492 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is dark blue colored. Applications: domestic water, heating, relining, plumbing, and in..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-6020 Polypropylene Random Copolymer
RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
|
|||
| Head Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Borealis RA130E-8427 Polypropylene Random Copolymer
RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Pipe Extrusion |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Pipe Extrusion |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||