Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 230 - 245 °C
446 - 473 °F
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v..
Head Temperature 230 - 245 °C
446 - 473 °F
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **)
Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and..
Head Temperature 230 - 245 °C
446 - 473 °F
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt ..
Head Temperature 230 - 245 °C
446 - 473 °F
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **)
Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g..
Head Temperature 230 - 240 °C
446 - 464 °F
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion
Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen..
Head Temperature 230 - 240 °C
446 - 464 °F
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating
Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c..
Head Temperature 230 °C
446 °F
Borealis ME6032 Polypropylene
ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S..
Head Temperature 230 °C
446 °F
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene
OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Head Temperature 230 - 250 °C
446 - 482 °F
Pipe Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..