Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre-drying |
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o.. |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre-drying |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Drying Temperature | 60.0 °C | 140 °F | |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Drying Temperature | 60.0 °C @Time >=10800 sec |
140 °F @Time >=3.00 hour |
If stored for longer than 1 year |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | Temperature can be reduced when using vacuum ovens. |
LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | Injection Molding |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection Molding |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | ( 2 hrs) Pre drying temp. |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Drying Temperature | 60.0 °C | 140 °F | |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI835H PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |