| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 90.0 °C | 194 °F | |
|
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Drying Temperature | 90.0 °C | 194 °F | |
|
Pasargad Polymer Peyvand Pasamid 3P-H1000W Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Drying Temperature |
90.0
°C <br>@Time 7200 sec
|
194
°F <br>@Time 2.00 hour
|
|
|
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||
| Drying Temperature | 90.0 °C | 194 °F | |
|
Pasargad Polymer Peyvand Pasamid 3P-H2000B1 Nylon 66
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Drying Temperature |
90.0
-
110
°C <br>@Time 14400 - 21600 sec
|
194
-
230
°F <br>@Time 4.00 - 6.00 hour
|
Pre-dry |
|
Kingfa PA66-RG001 Flame Retardant PA66
Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf..
|
|||
| Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
|
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
|
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
|
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 66 E21 PA 66, Impact Modified
Polyamide 66 (PA66). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
|
|||
| Drying Temperature |
90.0
-
105
°C <br>@Time 14400 - 21600 sec
|
194
-
221
°F <br>@Time 4.00 - 6.00 hour
|
Pre-dry |
|
Kingfa MAC-501DY Modified PC/ABS Alloy
Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
|
|||
| Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Predrying Temperature |
|
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Predrying Temperature |
|
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Drying Temperature | 90.0 °C | 194 °F | |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Drying Temperature | 90.0 °C | 194 °F | |
|
Pasargad Polymer Peyvand Pasamid 3P-M1000W Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
|
Asahi Kasei Xyron® 300V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
|
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
|
|||
| Drying Temperature |
90.0
-
100
°C <br>@Time 10800 sec
|
194
-
212
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||
| Drying Temperature |
90.0
°C <br>@Time 7200 sec
|
194
°F <br>@Time 2.00 hour
|
|
|
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||