Polymer Property : Shelf Life = 36.0 Month Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Dow Corning 805 RESIN
Silicone binder resin for maintenance paints, colored baking enamels, decorative finishes; primarily with metallic pigments. Used alone or blended with Dow Corning® 806A Resin to promote intermedia..
Shelf Life 36.0 Month
36.0 Month
Dow Corning 806A RESIN
Silicone binder resin for colored baking enamels for space heaters, stoves, etc. Used alone or blended with Dow Corning® 805 Resin to promote intermediate hardness.Information provided by Dow Corni..
Shelf Life 36.0 Month
36.0 Month
Dow Corning A Compound Antifoam
100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning ANTIFOAM C EMULSION, FOOD GRADE
Dow Corning Antifoam C Emulsion is a 30 percent food-grade silicone emulsion. This antifoam is water dilutable and effective in a variety of systems.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning FG-10 ANTIFOAM EMULSION
10 percent active, food-grade silicone emulsion designed to control foam in aqueous systems.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning H-10 ANTIFOAM EMULSION
10 percent active, water dilutable silicone emulsion designed to control foam in water based industrial processes.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning MOLYKOTE® G-0103 GREASE
Mineral base multi-service grease designed for extended lubrication of bearingsInformation provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® 99-595-HC LIQUID SILICONE RUBBER KIT
40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS 4-9038 FLUOROSILICONE RUBBER
50 Durometer, off-white, uncatalysed, high temperature grade fluorosilicone base.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS 5-2040 FLUOROSILICONE RUBBER
40 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS 5-2060 FLUOROSILICONE RUBBER
60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS 5-8761 FLUOROSILICONE RUBBER BASE
67 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS-2380 FLUOROSILICONE RUBBER
70 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SILASTIC® LS-2840 FLUOROSILICONE RUBBER
40 Durometer, off-white, uncatalysed, moulding grade fluorosilicone baseInformation provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning SYL-OFF® 297 ANCHORAGE ADDITIVE
Syl-Off® 297 Anchorage Additive is a mixture of reactive silanes that is used to improve abrasion resistance and adhesion of the cured coating to the substrate.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning XIAMETER® PMCPPMX-200 100,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 100,000CS. 100% active, 100,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6026 SILANE
Dow Corning® Z-6026 Silane is a chemically reactive material composed of an amino-alkyltrimethoxysilane and a polyol diluted to 40% by weight in methanol. Chemically, it is similar to Dow Corning®..
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6070 SILANE
Dow Corning Z-6070 Silane is a chemical monomer that reacts with water to form a silanetriol and methanol. The silanol that is formed is able to condense with available hydroxyl groups on the surfac..
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6124 SILANE
Dow Corning® Z-6124 Silane has the chemical formula: (CH3O)3Si and is designated phenyltrimethoxy silane. Dow Corning Z-6124 Silane is a chemical monomer that reacts with water to form a silanetrio..
Shelf Life 36.0 Month
36.0 Month
Dow Corning 1400 Antifoam
100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning XIAMETER® PMCPPMX-200 60,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 60,000CS. 100% active, 60,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6020 SILANE
Aminoethylaminopropyltrimethoxysilane - H2NC2H4NHC3H6-Si(OCH3)3 Coupling agent for many thermoset and thermoplastic resins with glass or mineral fillers.Information provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6040® SILANE
Dow Corning® Z-6040 Silane is a bifunctional silane containing a glycidoxy reactive organic group and a trimethoxysilyl inorganic group. It is designated ?-glycidoxypropyltrimethoxysilane. This gly..
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6042 SILANE
?-Glycidoxypropyl(methyl) diethoxysilaneInformation provided by Dow Corning
Shelf Life 36.0 Month
36.0 Month
Dow Corning Z-6106 SILANE
Dow Corning® Z-6106 Silane acts as a coupling agent designed to promote adhesion of two dissimilar materials. It can be used to bond a polymeric coating or adhesive to an inorganic substrate or to ..
Shelf Life 36.0 Month
36.0 Month
Dow Corning 2-5088 Wax
Silicone wax (siloxane backbone with pendant C30 alkyl groups attached). In home and auto care applications, it combines the shine and durability associated with hard waxes, with features closer to ..
Shelf Life 36.0 Month

@Temperature 7.22 °C
36.0 Month

@Temperature 45.0 °F
From date of manufacture
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,..
Shelf Life 36.0 Month

@Temperature 15.0 - 27.0 °C
36.0 Month

@Temperature 59.0 - 80.6 °F
3M PN8017 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shelf Life 36.0 Month

@Temperature 15.0 - 27.0 °C
36.0 Month

@Temperature 59.0 - 80.6 °F
3M PN8019 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shelf Life 36.0 Month
36.0 Month
Dow Corning 3074 INTERMEDIATE
Reactive silicone intermediate for coil coatings, appliance finishes and other finishes where improved heat or weathering resistance is needed. Typically reacted with saturated polyesters to form si..