Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.116666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min @Temperature 193 °C |
0.116666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min @Temperature 379 °F |
hot plate |
3M Scotchcast™ 263 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |