Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcast™ 263 Electrical Epoxy Powder Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer 3M
Trade Name Scotchcast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 263 Electrical Epoxy Powder Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dialectic coating to a variety of substrates. It is intended for use where high temperature cut-through resistant is required. Scotchcast Electrical Resin 263 is manufactured by a fusion blend process, ensuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Scotchcast 263 is applied to an object that has been heated to a temperature above the melting point of the resin. On contact with the preheated application surface, the resin melts, flows to a controlled extent, then cures, bonding to the substrate and coalescing into a smooth, continuous, essentially uniform thick coating. It effectively coats flat surfaces and corners, as well as, high point. Uses for Scotchcast 263 include moisture proofing and insulating armatures, stators, buss bars and toroid cores.Information provided by 3M
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
cured; ASTM D794
Mechanical Properties Metric English Comments
Impact Test 11.3 J
8.33 ft-lb
12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Abrasion 0.60
0.60
[g] Removed from 12-15 mil coating; ASMT D4060
Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm
1000 kV/in
12 to 15 mil coating; ASTM D149
Processing Properties Metric English Comments
Cure Time 0.333 min

@Temperature 232 °C
0.00556 hour

@Temperature 450 °F
0.500 min

@Temperature 204 °C
0.00833 hour

@Temperature 399 °F
10.0 min

@Temperature 177 °C
0.167 hour

@Temperature 351 °F
30.0 min

@Temperature 149 °C
0.500 hour

@Temperature 300 °F
Gel Time 0.116666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.116666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
Shelf Life 24.0 Month

@Temperature <=27.0 °C
24.0 Month

@Temperature <=80.6 °F
Descriptive Properties Value Comments
Appearance Green