| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | IEC 60093 |
|
Murtfeldt Murflor® Polytetrafluoroethylene
Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
|
|||
| Electrical Resistivity | 1.00e+17 - 2.60e+17 ohm-cm | 1.00e+17 - 2.60e+17 ohm-cm | Average value: 2.13e+17 ohm-cm Grade Count:6 |
|
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
|
|||
| Electrical Resistivity | 1e+05 - 1.00e+17 ohm-cm | 1e+05 - 1.00e+17 ohm-cm | Average value: 1.68e+16 ohm-cm Grade Count:58 |
|
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
|
|||
| Electrical Resistivity | 1e+05 - 1.00e+17 ohm-cm | 1e+05 - 1.00e+17 ohm-cm | Average value: 9.72e+15 ohm-cm Grade Count:24 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
|
|||
| Electrical Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | Average value: 9.55e+17 ohm-cm Grade Count:10 |
|
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 100A Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 200FPC Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thickn..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 |
|
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).Genera..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available ..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 50KN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
|
DuPont™ Kapton® 200KN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianh..
|
|||
| Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber
This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform..
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
|
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||