| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IEC 60093 |
|
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
|
|||
| Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53 482 |
|
Perstorp Compounds 171 Urea-Formaldehyde w/ cellulose filler
Information provided by Perstorp Compounds Inc.
|
|||
| Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53 482 |
|
Perstorp Compounds Aminel FX Melamine
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp ..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
|
|||
| Surface Resistance | 1.00e+11 - 1.00e+17 ohm | 1.00e+11 - 1.00e+17 ohm | Average value: 9.84e+15 ohm Grade Count:11 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti
Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application ..
|
|||
| Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
|
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control..
|
|||
| Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
|
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is ..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 GF33 LE 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Extraction ResistantProcessing Method: Injection MoldingInformation provided b..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® HT XE 3996 PA*-GF30
Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® TSM-40/4 PA666-MD40
Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® TSS/4 LF 1 PA666
Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® XE 4071 black 9992 PA612
Product description: Grilamid XE 4071 BLACK 9992 is an impact modified unreinforced high viscosity polyamide 612 (PA612) extrusion grade with superior heat and hydrolysis resistance. Compared to sta..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
|
EMS-Grivory Grivory® L 25 W 40 PA12
Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid ..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | CEI 60093 |
|
Addiplast Addilene H 530 N30 Polypropylene Homopolymer
Good surface appearanceInformation provided by Addiplast.
|
|||
| Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | IS 3396-1979 |
|
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | |
|
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Conditioned; CEI 60093 |
|
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled
Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast.
|
|||
| Surface Resistance | 1.00e+11 - 3.16e+11 ohm | 1.00e+11 - 3.16e+11 ohm | IS 3396-1979 |
|
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
|
Techmer ES Statiblend® PP FR BK
Availability: North AmericaForms: PelletsFeature: Flame Retardant, Homopolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
|
|||
| Surface Resistance |
<=
1.00e+11
ohm <br>@Time 86400 sec
|
<=
1.00e+11
ohm <br>@Time 24.0 hour
|
1% dosing rate |
|
Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based
Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications..
|
|||
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Conditioned; CEI 60093 |
|
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
|
|||