| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced
(discontinued **)
Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo..
|
|||
| Arc Resistance | 185 - 190 sec | 185 - 190 sec | ASTM D495 |
|
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-7-120NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance moldi..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | ASTM D495 |
|
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | ASTM D495 |
|
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | ASTM D495 |
|
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | ASTM D495 |
|
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | ASTM D495 |
|
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
IDI Composites E-203 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact
Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Industrial Laminates/Norplex MC511A Glass Fabric
Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3)
ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy
E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Plenco 6015 Phenolic, Briquette, Injection Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Plenco 6990 Phenolic, Briquette, Injection Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Plenco 6990 Phenolic, Briquette, Transfer Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | |
|
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
|
|||
| Arc Resistance | 185 sec | 185 sec | |
|
Bulk Molding Compounds BMC 1050 Thermoset Polyester
BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e..
|
|||
| Arc Resistance | 185 sec | 185 sec | |
|
Bulk Molding Compounds BMC 1410 Electrical Grade
BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | |
|
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel..
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | |
|
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester
BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in ..
|
|||
| Arc Resistance | 185 sec | 185 sec | |
|
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
Sumitomo Bakelite North America RX® 865M Novolac Phenolic
Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group
|
|||
| Arc Resistance | >= 185 sec | >= 185 sec | |
|
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
|
|||
| Arc Resistance | 185 sec | 185 sec | ASTM D495 |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical
|
|||