| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | |
| Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC 60 Hz |
| Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC 60 Hz |
| Fujipoly Industries Sarcon® 20GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC 60 Hz |
| Fujipoly Industries Sarcon® 20GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | 150°C for 1,000 hrs |
| Fujipoly Industries Sarcon® 20GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | 60°C for 500 hrs |
| Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | 60°C for 500 hrs |
| Fujipoly Industries Sarcon® 30T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | 200°C for 1,000 hrs |
| Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | 60°C for 500 hrs |
| Fujipoly Industries Sarcon® 85H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | Step by Step; ASTM D149 |
| Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC Rapid Rise; ASTM D149 |
| DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC Rapid Rise; ASTM D149 |
| DuPont™ Nomex® N196 Paper, 15 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC Rapid Rise; ASTM D149 |
| DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | AC Rapid Rise; ASTM D149 |
| DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
| Dielectric Strength | 6.00 - 8.00 kV/mm @Temperature 90.0 °C |
152 - 203 kV/in @Temperature 194 °F |
IS 2584-1963 |
| Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
| Dielectric Strength | 6.00 - 8.00 kV/mm @Temperature 90.0 °C |
152 - 203 kV/in @Temperature 194 °F |
IS 2584-1963 |
| Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | dry; IEC 60243-1 |
| EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
| Dielectric Strength | 6.00 kV/mm | 152 kV/in | conditioned; IEC 60243-1 |
| EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
| Dielectric Strength | 6.00 - 35.0 kV/mm | 152 - 889 kV/in | Average value: 20.3 kV/mm Grade Count:3 |
| Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||