Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 65.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir ICE R 830D Polystyrene
Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir R 540E Polystyrene
HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection moldings. Designation: Thermoplastics IS..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir R 850E Polystyrene
Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even diluted with high percentage of GP. Suitable for general injecti..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir RT 461F Polystyrene
High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR
Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir RC 600 Polystyrene
Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir RCL 600 Polystyrene  (discontinued **)
Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60243
Polimeri Europa Edistir ICE S 800/N Polystyrene  (discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
Dielectric Strength 65.0 kV/mm
1650 kV/in
Polimeri Europa EDISTIR PD RK4514H High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,093-06-07-23 UL94 V-2, polybromodiphenylether (PBBE) free, antimony free, HIPS satisfying at 960°C the glow wire test..
Dielectric Strength 65.0 kV/mm
1650 kV/in
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r..
Dielectric Strength 65.0 kV/mm
1650 kV/in
Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,093-06-07-12 Very high environmental stress cracking resistant (VH ESCR) modified HIPS. It exhibits high toughness and ..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IPC-TM-650.2.5.6.2
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
Dielectric Strength 65.0 kV/mm
1650 kV/in
200µm film; IEC 60243-1
3M Dyneon™ TFM™ 1605 Modified PTFE Powder  (discontinued **)
Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon.
Dielectric Strength 65.0 kV/mm
1650 kV/in
Saint-Gobain CHR® 2042-10 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Strength 65.0 kV/mm
1650 kV/in
VDE 0303/4
Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant
30% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..
Dielectric Strength 65.0 kV/mm
1650 kV/in
IEC 60250
Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized
45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.Information provided by Polyram.
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Dielectric Strength 65.0 kV/mm
1650 kV/in
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI..
Dielectric Strength 65.0 - 146 kV/mm
1650 - 3710 kV/in
Average value: 75.1 kV/mm Grade Count:8
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Dielectric Strength 65.0 kV/mm
1650 kV/in
ASTM D149
Mitsui TPX® DX820 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..