Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 1.00e+9 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+9 ohm-cm
>= 1.00e+9 ohm-cm
ASTM D257-91
NeXolve LaRC™-CP1 Polyimide
Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak..
Volume Resistivity 1e+05 - 1.00e+9 ohm-cm
1e+05 - 1.00e+9 ohm-cm
ASTM D257
Haysite SDL® H400 Polyester Composite
H400 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H400..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
Volume Resistivity 1.00e+9 - 1.00e+10 ohm-cm
1.00e+9 - 1.00e+10 ohm-cm
ASTM D257
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene
Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C..
Volume Resistivity 1.00e+9 - 1.00e+11 ohm-cm
1.00e+9 - 1.00e+11 ohm-cm
Dry; ASTM D257
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)
Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Practical Use (Water Absorption 2.1%); ASTM-D257
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+9 - 1.00e+10 ohm-cm
1.00e+9 - 1.00e+10 ohm-cm
Practical Use (Water Absorption 2.5%); ASTM-D257
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
IEC 60093
BASF Ultramid® C3U PA66/6 (Conditioned)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
IEC 60093
BASF Ultramid® A3W PA66 (Conditioned)
Description: Free-flowing, heat aging resistant and rapidly processable grade for technical parts subject to high stress such as bearings and bearing cages, gearwheels and spool bodies.Information p..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
IEC 60093
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Practical Use (Water Absorption 2.8%); ASTM-D257
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Adamas Adalon® 305 PTFE, 15% Graphite
Information provided by Adamas, HPM