Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Clariant > Category : Polymer Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Nylon 6, 10% Glass Fiber Filled
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced Nylon 6, 10% Glass Fiber Filled
Clariant 6008 L Nylon 6, High Impact, Injection Molding Nylon 6, Impact Grade
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Nylon 612
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Nylon 66
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Nylon 66, 20% Glass Fiber Filled
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 66, 40% Glass Fiber Filled
Clariant ABS4500 ABS, High Impact Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Clariant ABS4500G10BK ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Clariant ABS4500G30 ABS, 30% Glass Reinforced Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Clariant ABSSP0004 ABS, Chemical Resistant ABS Polymer
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Nylon 66
Clariant CA9000NAT` Acetal Copolymer Acetal Copolymer, Unreinforced
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Thermoplastic Polyurethane (TPUR), Polyether Grade
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, 20% Glass Fiber Filled
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant PA131 Nylon 66, Highly Impact Modified Nylon 66, Impact Grade
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Nylon 66
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Nylon 6, 40% Mineral Filled
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Nylon 6, 40% Mineral Filled
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Nylon 6, Glass/Mineral Reinforced
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Nylon 6
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified Nylon 612, Glass Fiber Filler
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified Nylon 612, Glass Fiber Filler
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Polycarbonate, Stainless Steel Fiber
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled LLDPE
Clariant Remafin PP1100NAT Polypropylene Impact Modified Copolymer Polypropylene Copolymer
Clariant Renol 6001 GP HSL Nylon 6, Heat Stabilized, Lubricated Nylon 6, Heat Stabilized
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated Nylon 6, Heat Stabilized
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Nylon 6, MoS2 Filled
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 6, 10% Glass Fiber Filled
Clariant Renol 60G33HSL Nylon 6, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 6, 30% Glass Fiber Filled
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated Nylon 6, 30% Glass Fiber Filled
Clariant Renol 612-01L Nylon 612, Lubricated Nylon 612
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated Nylon 612, Glass Fiber Filler
Clariant Renol 612G20-L Nylon 612, 20% Glass Fiber Reinforced, Lubricated Nylon 612, Glass Fiber Filler
Clariant Renol 6253 Nylon 6, High Impact Nylon 6, Impact Grade
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Nylon 6, Impact Grade
Clariant Renol 6601FR Nylon 66, Flame Retardant Nylon 66, Unreinforced, Flame Retardant
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced Nylon 66, 20% Glass Fiber Filled
Clariant Renol 66G33 2% Moly Nylon 66, 33% Glass Fiber Reinforced, 2% Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 66, 30% Glass Fiber Filled
Clariant Renol ABNN732017 Nylon 6 with anchored silicone Nylon 6
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss ABS Polymer
Clariant Renol ABS3470 ABS, High Heat, Low Gloss ABS Polymer
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss ABS Polymer
Clariant Renol BR2025 Nylon 66, Impact Modified Nylon 66, Impact Grade
Clariant Renol BR2029 Nylon 66, General Purpose, Black Nylon 66
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Nylon 66, Glass/Mineral Filled
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Nylon 66, PTFE Filled
Clariant Renol BR4014BK ABS, High Gloss, Black ABS Polymer
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Polycarbonate/PET Polyester Blend
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU Nylon 6
Clariant Renol BR7039G30 Nylon 6, 30% Glass Fiber, bondable to TPU Nylon 6, 30% Glass Fiber Filled
Clariant Renol BR7140 Polycarbonate/ABS Alloy Polycarbonate/ABS Alloy, Unreinforced
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Nylon 66
Clariant Renol CAB1000 Cellulose Acetate Butyrate Cellulose Acetate Butyrate, Molded
Clariant Renol CP-MF-9 Acetal Copolymer Acetal Copolymer, Unreinforced
Clariant Renol CPS04230 Color concentrate of Titanium Oxide Additive/Filler for Polymer
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated Nylon 6, Impact Grade
Clariant Renol PA101L Nylon 66, General Purpose, Lubricated Nylon 66
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Nylon 66
Clariant Renol PA111 Nylon 66, General Purpose Nylon 66
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Nylon 66, Glass/Carbon Fiber Filled
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow Nylon 66, 40% Glass Fiber Filled
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Nylon 66, 50% Glass Fiber Filled
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow Nylon 66, 50% Glass Fiber Filled
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Nylon 66, 60% Glass Fiber Filled
Clariant Renol PA112 Nylon 66, Nucleated Nylon 66, Nucleated
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol PA113G13 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber Nylon 66, 20% Glass Fiber Filled
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Nylon 66, Heat Stabilized
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black Nylon 66
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Nylon 66, 30% Glass Fiber Filled
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Nylon 66/6, 10% Glass Fiber Reinforced
Clariant Renol PA1SP0003 Nylon 66, PE Modified Nylon 66
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD Nylon 66, Impact Grade
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Nylon 66, Glass Reinforced, Impact Grade
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Clariant Renol PA211 Nylon 6, General Purpose Nylon 66, Heat Stabilized
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber Nylon 6, 10% Glass Fiber Filled
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Nylon 6, 40% Glass Fiber Filled
Clariant Renol PA211G50 Nylon 6, 50% Glass Fiber, Lubricated Nylon 6, 50% Glass Fiber Filled
Clariant Renol PA211N40 Nylon 6, Mineral/Glass Fiber, Heat Stabilized, Lubricated Nylon 6, Glass/Mineral Reinforced
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Nylon 6, Heat Stabilized
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated Nylon 6, 10% Glass Fiber Filled
Clariant Renol PA213G15 Nylon 6, 15% Glass Fiber, Heat Stabilized, Lubricated Nylon 6, 20% Glass Fiber Filled
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated Nylon 6, 30% Glass Fiber Filled
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Nylon 6, 30% Glass Fiber Filled
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated Nylon 6, 40% Glass Fiber Filled
Copyright © lookpolymers.com All Rights Reserved