| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled |
| Manufacturer | Clariant |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
| Elongation at Yield | 15 % | 15 % | ASTM D638 |
| Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
| Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
| Izod Impact, Notched | 0.374 J/cm @Temperature 22.8 °C |
0.700 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
| Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
| Dry Time | 2 - 4 hour @Temperature 79.4 °C |
2 - 4 hour @Temperature 175 °F |
to ensure moisture level is less than 0.2% |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |