PRODUCT NO. Category Trade Name
DSM Akulon® CO-KGV4 /A JN.00.86 PA6-GF20 FR Nylon 6, Glass Fiber Filled, Flame Retardant Akulon®
DSM Akulon® F126-C Nylon 6 (European Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® F127 PA6 Film Akulon®
DSM Akulon® F130 PA6 Film Akulon®
DSM Akulon® F130-C PA6 Film Akulon®
DSM Akulon® F130-C2 PA6 Film Akulon®
DSM Akulon® F130-C3 PA6 Nylon 6, Film Grade Akulon®
DSM Akulon® F130-E1 PA6 Film Akulon®
DSM Akulon® F130-E5 PA6 Film Akulon®
DSM Akulon® F132 PA6 Film Akulon®
DSM Akulon® F132-C1 PA6 Film Akulon®
DSM Akulon® F132-E1 PA6 Film Akulon®
DSM Akulon® F132-E2 PA6 Film Akulon®
DSM Akulon® F136 PA6 Film Akulon®
DSM Akulon® F136-C PA6 Film Akulon®
DSM Akulon® F136-C1 PA6 Film Akulon®
DSM Akulon® F136-DH Nylon 6 (European Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® F136-E1 PA6 Film Akulon®
DSM Akulon® F136-E2 PA6 Film Akulon®
DSM Akulon® F150-CZ PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® F160-Z PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America) Nylon 6, Unreinforced Akulon®
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America) Nylon 6, Unreinforced Akulon®
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) Nylon 6, Unreinforced Akulon®
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® F230-C PA6 Film Akulon®
DSM Akulon® F232 PA6 Film Akulon®
DSM Akulon® F232-D Nylon 6 (European Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® F234-C PA6 Nylon 6, Film Grade Akulon®
DSM Akulon® F236-C Nylon 6 (European Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® Fuel Lock FL-LP PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® F-X9182 PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® F-X9183 PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® F-X9215 PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® K123, K123/A PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® K125 PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® K125/A PA6 Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-D (Cond.) Low Viscosity Nylon 6 (North America) Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-D (Dry) Low Viscosity Nylon 6 (North America) Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Cond) Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Dry) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K222-KGV5 Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K223-HGM24 Nylon 6-30% Glass and Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K223-HGM24 Nylon 6-30% Glass and Mineral Reinforced (European and Asian Grade) (Dry) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Cond) Nylon 6, Impact Grade Akulon®
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Dry) Nylon 6, Impact Grade Akulon®
DSM Akulon® K224-G0 (Cond.) 50% Glass Reinforced Nylon 6 (North America) Nylon 6, 50% Glass Fiber Filled Akulon®
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) Nylon 6, 50% Glass Fiber Filled Akulon®
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) Nylon 6, 50% Glass Fiber Filled Akulon®
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-G4U (Cond.) 23% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6-FC BK00001 PA6-GF30 Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6-FC NA99001 PA6-GF30 Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-G8 PA6-GF40 Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG3 (Cond.) 15% Glass Reinforced Nylon 6 (North America) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6 (Dry) 30% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG7 (Cond.) 35% Glass Reinforced Nylon 6 (North America) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® K224-HGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K224-LG6 /E PA6-GF30 Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-LGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K224-LGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Nylon 6, Glass/Mineral Reinforced Akulon®
DSM Akulon® K224-PG2 PA6-I-GF8 Nylon 6, 10% Glass Fiber Filled Akulon®