| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Akulon® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Akulon® K125/A PA6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | dry; ISO 1183 |
| Water Absorption | 9.5 % | 9.5 % | Sim. To ISO 62 |
| Moisture Absorption | 2.50 % | 2.50 % | Sim. To ISO 62 |
| Viscosity Test | 152 cm³/g | 152 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | cond; ISO 527-1/-2 |
| 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 20 % | 20 % | dry; ISO 527-1/-2 |
| >= 50 % | >= 50 % | cond; ISO 527-1/-2 | |
| Elongation at Yield | 4.0 % | 4.0 % | dry; ISO 527-1/-2 |
| 25 % | 25 % | cond; ISO 527-1/-2 | |
| Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
| 3.20 GPa | 464 ksi | dry; ISO 527-1/-2 | |
| Flexural Strength | 100 MPa | 14500 psi | dry; ISO 178 |
| Flexural Modulus | 2.60 GPa | 377 ksi | dry; ISO 178 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
cond; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
cond; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
dry; ISO 179/1eU | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
dry; ISO 179/1eU | |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
| 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA | |
| 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA | |
| 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |