Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : EMS-Grivory (EMS-CHEMIE) Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
EMS-Grivory Grivory® 1S XE 4224 nat PA1010 Nylon Grivory®
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Renewable/Recycled Polymer Grivory®
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Renewable/Recycled Polymer Grivory®
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Renewable/Recycled Polymer Grivory®
EMS-Grivory Grivory® AG-35 PA66-GF35 Nylon 66, 30% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR Nylon 6, 30% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Nylon 6, 30% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® BG-35 S PA6-GF35 Nylon 6, 40% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Nylon 6, Glass/Mineral Reinforced Grivory®
EMS-Grivory Grivory® BK-50 PA6-GB50 Nylon 6, Glass Bead Filled Grivory®
EMS-Grivory Grivory® BM-30 PA6-MD30 Nylon 6, 30% Mineral Filled Grivory®
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15 Nylon 66/6, 20% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Nylon 6, 20% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® F 34 NL PA6 Nylon 6 Grivory®
EMS-Grivory Grivory® GV-5H black PA*-GF50 Nylon Grivory®
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Nylon Grivory®
EMS-Grivory Grivory® HB5299 PA* Nylon Grivory®
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Renewable/Recycled Polymer Grivory®
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Nylon 6/66 Grivory®
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30 Nylon Grivory®
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40 Nylon 66, 40% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Nylon 66, 50% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® L 20A Z PA12 Nylon 12 Grivory®
EMS-Grivory Grivory® L 25H FWA black 9225 PA12 Nylon 12 Grivory®
EMS-Grivory Grivory® LKN-5H PA12-GB50 Nylon 12, Glass Bead Filled Grivory®
EMS-Grivory Grivory® LV-23H PA12-GF23 Nylon 12, 20% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® LV-5H PA12-GF50 Nylon 12, 50% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Nylon 6/66 Grivory®
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Nylon 66/6, 40% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Nylon 66/6, 40% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Nylon 66/6, 40% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Nylon 66/6, 30% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® TSM-30 PA666-MD30 Nylon 66/6, Mineral Reinforced Grivory®
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI Nylon 12 Grivory®
EMS-Grivory Grivory® XE 4073 nat PA610 Renewable/Recycled Polymer Grivory®
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Nylon Grivory®
EMS-Grivory Grivory® XE 4105 black 9992 PA610-GF50 Nylon 610, Glass Reinforced Grivory®
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Nylon Grivory®
EMS-Grivory Grivory® BG-50 PA6-GF50 Nylon 6, 50% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® GV-4H PA*-GF40 Nylon Grivory®
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Nylon 6/66 Grivory®
EMS-Grivory Grivory® L 25 H PA12 Nylon 12 Grivory®
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Nylon 12, 30% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Nylon Grivory®
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Nylon 66/6, 30% Glass Fiber Reinforced Grivory®
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Nylon 66, 30% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® LC-15H black PA12-CF15 Nylon 12, Carbon Fiber Filled Grivory®
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Nylon 12, 50% Glass Fiber Filled Grivory®
EMS-Grivory Grivory® TS FR PA666 FR Nylon 6/66 Grivory®
Copyright © lookpolymers.com All Rights Reserved