| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
| Water Absorption | 7.0 % | 7.0 % | ISO 62 |
| Moisture Absorption | 2.50 % | 2.50 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 70.0 MPa | 10200 psi | conditioned; ISO 2039-1 |
| 165 MPa | 23900 psi | dry; ISO 2039-1 | |
| Tensile Strength at Break | 60.0 MPa | 8700 psi | conditioned; ISO 527-1/-2 |
| 100 MPa | 14500 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 6.0 % | 6.0 % | dry; ISO 527-1/-2 |
| 50 % | 50 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 4.50 GPa | 653 ksi | conditioned; ISO 527-1/-2 |
| 7.00 GPa | 1020 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | dry; ISO 179/1eU |
| NB | NB | conditioned; ISO 179/1eU | |
| 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| 5.00 J/cm² @Temperature 30.0 °C |
23.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | dry; ISO 179/1eA |
| 0.600 J/cm² | 2.86 ft-lb/in² | conditioned; ISO 179/1eA | |
| 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
| 160 °C | 320 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-2 | V-2 | IEC 60695-11-10 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Electricals & Electronics | Connectors | |
| Electrical equipment | ||
| Energy distribution | ||
| Form | Granules | |
| Processing | Injection Molding | |
| Special Characteristics | Flame retardant |