Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Freudenberg Simrit > Category : Polymer Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Freudenberg Simrit 92 AU 21100 Low Temperature Polyurethane Elastomer Thermoset Polyurethane, Elastomer, Unreinforced
Freudenberg Simrit E425 Hydrocarbon Elastomer Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit F40 Fluorosilicone Elastomer Thermoset Fluoroelastomer
Freudenberg Simrit F70 Fluorosilicone Elastomer Thermoset Fluoroelastomer
Freudenberg Simrit F80 Fluorosilicone Elastomer Thermoset Fluoroelastomer
Freudenberg Simrit Hydrolysis-Resistant Polyurethane Elastomer Thermoset Polyurethane, Elastomer, Unreinforced
Freudenberg Simrit N431 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N432 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N442 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N445 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S310 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S313 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S314 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S315 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S40 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S40GY Silicone Elastomer Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S50 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S70 Silicone Elastomer Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S70 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S80 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit SC1210 S310 Silicone Elastomer Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit SC1217 S317 Silicone Elastomer Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 484 FDA FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 485 Universal FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 486 Universal FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 487 High Temperature FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 488 High Temperature FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Simriz® 489 Ultra Pure FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit Superiorâ„¢ F815 Fluoroelastomer Thermoset Fluoroelastomer Superior™
Freudenberg Simrit Superiorâ„¢ F850 Fluoroelastomer Thermoset Fluoroelastomer Superior™
Freudenberg Simrit V115 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V121 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V141 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V158 Fluoroelastomer Self-Lube Thermoset Fluoroelastomer
Freudenberg Simrit V160 Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V169 Fluoroelastomer Self-Lube Thermoset Fluoroelastomer
Freudenberg Simrit V174 Fluoroelastomer Self-Lube Thermoset Fluoroelastomer
Freudenberg Simrit V175 Aflasâ„¢ (TFE/P) Thermoset Fluoroelastomer
Freudenberg Simrit V176 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V177 Fluoroelastomer Self-Lube Thermoset Fluoroelastomer
Freudenberg Simrit V178 Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V180 Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V189 Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V195 Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V60 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V60WH Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V75BR Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V75WH Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit V90BR Non-Black Compound Thermoset Fluoroelastomer
Freudenberg Simrit N456 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N466 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N470 Hydrocarbon Elastomer Nitrile Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N470 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit N475 Nitrile Elastomer (NBR) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit S60 Silicone Elastomer (VMQ) Rubber or Thermoset Elastomer (TSE)
Freudenberg Simrit Simriz® 482 Low Temperature FFKT Perfluoroelastomer Compound Thermoset Fluoroelastomer Simriz®
Freudenberg Simrit V123 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit V75 Standard Fluoroelastomer Thermoset Fluoroelastomer
Freudenberg Simrit Viton® SC1106 CV75 ETP Thermoset Fluoroelastomer Viton®
Freudenberg Simrit Viton® SC1106 CV75 HP-1 (TFE/P) Thermoset Fluoroelastomer Viton®
Freudenberg Simrit Viton® SC1107 CV75WH ETP Thermoset Fluoroelastomer Viton®