| LyondellBasell Alathon® ETP H4745 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon® ETP
|
| LyondellBasell Alathon® ETP H4837 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon® ETP
|
| LyondellBasell Alathon® ETP H5057 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon® ETP
|
| LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® H5520 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® H6018 High Density Polyethylene (Extrusion Grade) |
High Density Polyethylene (HDPE), Extruded |
Alathon®
|
| LyondellBasell Alathon® H6018 High Density Polyethylene (Film Grade) |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® H6030 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® L4903 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade |
High Density Polyethylene (HDPE), Pipe Grade |
Alathon®
|
| LyondellBasell Alathon® L5008 High Density Polyethylene |
High Density Polyethylene (HDPE), Pipe Grade |
Alathon®
|
| LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade |
High Density Polyethylene (HDPE), Pipe Grade |
Alathon®
|
| LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade |
High Density Polyethylene (HDPE), Blow Molding Grade |
Alathon®
|
| LyondellBasell Alathon® L5045 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® L5332CP High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Alathon®
|
| LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade |
High Density Polyethylene (HDPE), Blow Molding Grade |
Alathon®
|
| LyondellBasell Alathon® L5440 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
Alathon®
|
| LyondellBasell Alathon® L5485 High Density Polyethylene |
Film |
Alathon®
|
| LyondellBasell Alathon® L5840 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
Alathon®
|
| LyondellBasell Alathon® L5845 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® L5906 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® M4612 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M4621 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M4661 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M5040 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M5370 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade |
High Density Polyethylene (HDPE), Pipe Grade |
Alathon®
|
| LyondellBasell Alathon® M5370WC High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Alathon®
|
| LyondellBasell Alathon® M5372 High Density Polyethylene |
HDPE |
Alathon®
|
| LyondellBasell Alathon® M5562 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® M6020 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® M6028 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M6030 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® M6060 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
Alathon®
|
| LyondellBasell Alathon® M6061 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M6080WC High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Alathon®
|
| LyondellBasell Alathon® M6138 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Alathon® M6580 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Alathon®
|
| LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound |
High Density Polyethylene (HDPE), Crosslinkable |
Aquathene®
|
| LyondellBasell Lupolen® 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade |
High Density Polyethylene (HDPE), Pipe Grade |
Lupolen®
|
| LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade |
High Density Polyethylene (HDPE), Pipe Grade |
Lupolen®
|
| LyondellBasell Microthene® F FA70000 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Microthene® F
|
| LyondellBasell Microthene® F FA70900 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Microthene® F
|
| LyondellBasell Microthene® F FN50100 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® F
|
| LyondellBasell Microthene® F FN51000 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® F
|
| LyondellBasell Microthene® F FN51900 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® F
|
| LyondellBasell Microthene® G MN70100 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® G
|
| LyondellBasell Microthene® G MN71020 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® G
|
| LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) |
Low Density Polyethylene (LDPE), Molded |
Microthene® G
|
| LyondellBasell Microthene® G MN71400 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® G
|
| LyondellBasell Microthene® G MN72700 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Microthene® G
|
| LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Microthene®
|
| LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Microthene®
|
| LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film) |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film) |
Linear Low Density Polyethylene (LLDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Petrothene®
|
| LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Petrothene®
|
| LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Petrothene®
|
| LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene |
Film |
Petrothene®
|
| LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene |
Film |
Petrothene®
|
| LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene |
Film |
Petrothene®
|
| LyondellBasell Petrothene® GA616050 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Extrusion Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade |
Linear Low Density Polyethylene (LLDPE), Injection Molded |
Petrothene®
|
| LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene |
LLDPE |
Petrothene®
|
| LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene |
Low Density Polyethylene (LDPE), Extrusion Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Extrusion Grade |
Petrothene®
|
| LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Extrusion Grade |
Petrothene®
|
| LyondellBasell Petrothene® HR92953 Medium Density Polyethylene |
Medium Density Polyethylene (MDPE), Extruded |
Petrothene®
|
| LyondellBasell Petrothene® KR92717 High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Petrothene®
|
| LyondellBasell Petrothene® KR92828 High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Petrothene®
|
| LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade |
Low Density Polyethylene (LDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® LB5604 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LB560401 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LM600500 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LP5002 High Density Polyethylene (Blow Molding Grade) |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade) |
High Density Polyethylene (HDPE), Sheet/Thermoforming Grade |
Petrothene®
|
| LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade) |
High Density Polyethylene (HDPE), Sheet/Thermoforming Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade) |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) |
High Density Polyethylene (HDPE), Sheet/Thermoforming Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade) |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR732031 High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
Petrothene®
|
| LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) |
High Density Polyethylene (HDPE), Blow Molding Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) |
High Density Polyethylene (HDPE), Extruded |
Petrothene®
|
| LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade |
High Density Polyethylene (HDPE), Film Grade |
Petrothene®
|
| LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) |
High Density Polyethylene (HDPE), Extruded |
Petrothene®
|