Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5906 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5906 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high tensile strength, and low gels. Opportunities for this type of product include paper replacement applications as well as mono-and multi-layer films requiring both stiffness and toughness.Regulatory StatusXL 5906meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing XL 5906 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion ConditionsBUR=4:1, Neck Height= 6 Die Diameters, 0.5 Mil Film, Melt Temperature= 390°-410°F(199°-210°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
ASTM D792
Melt Flow 0.057 g/10 min
0.057 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 38.6 MPa
5600 psi
ASTM D822
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D822
Film Elongation at Break, MD 300 %
300 %
ASTM D822
Film Elongation at Break, TD 350 %
350 %
ASTM D822
Dart Drop, Total Energy 2.44 J
1.80 ft-lb
ASTM D3420
Elmendorf Tear Strength MD 10 g
10 g
ASTM D1922
Elmendorf Tear Strength TD 34 g
34 g
ASTM D1922
Film Tensile Strength at Break, MD 84.8 MPa
12300 psi
ASTM D822
Film Tensile Strength at Break, TD 64.5 MPa
9360 psi
ASTM D822
1% Secant Modulus, MD 1250 MPa
181000 psi
ASTM D822
1% Secant Modulus, TD 1280 MPa
186000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Typical Extrusion