| Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet |
Polypropylene, Extrusion Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH110 Polypropylene, Homopolymer, BCF |
Polypropylene, Fiber Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH120 Polypropylene, Homopolymer, Injection Molding, Barefoot |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH120LN Polypropylene, Homopolymer, Injection Molding, Antistat/Lube |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH180V Polypropylene, Homopolymer, BCF, UV, Gas Fading |
Polypropylene, Fiber Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH200L Polypropylene, Homopolymer, CR, Antistat, Injection Molding |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH350LN Polypropylene, Homopolymer, High Flow, Nucleated, Lube, Injection Molding |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH350V Polypropylene, Homopolymer, Extrusion Coating, Spunbound, Gas Fade & UV Resistant |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM100LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM120LN Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR120CL-01 Polypropylene, Random Copolymer, Clarified |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR350CL Polypropylene, Random Copolymer, Clarified, Lubricated |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR350CL-01 Polypropylene, Random Copolymer, Clarified |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR350LN Polypropylene, Random Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH005 Polypropylene, Homopolymer, Extrusion, Strapping |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film |
Film |
COPYLENE®
|
| Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH020S Polypropylene, Homopolymer, BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH034EW Polypropylene, Homopolymer, Slit Film, LWCO |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH042L Polypropylene, Homopolymer, Straw and Extrusion, Antistat |
Polypropylene, Extrusion Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH043L Polypropylene, Homopolymer, Lube, Straw |
Polypropylene, Extrusion Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH080V Polypropylene, Homopolymer, BCF Staple, UV |
Polypropylene, Fiber Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH085 Polypropylene, Homopolymer, Cast Film |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH200LN Polypropylene, Homopolymer, CR, Antistat, Nucleated, Injection Molding |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CM003P Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM020N Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM200LN Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR030LN Polypropylene, Mini-Random Copolymer, Thermoforming |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CH016 Polypropylene, Homopolymer, BOPP |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH034EV Polypropylene, Homopolymer, Fiber, Tape, UV |
Polypropylene, Fiber Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH034W Polypropylene, Homopolymer, Slit Film, LWCO |
Polypropylene, Film Grade |
COPYLENE®
|
| Phillips 66 COPYLENE® CH200LN-02 Polypropylene, Homopolymer, Rx grade, Nucleated, Lube, Injection Molding |
Polypropylene (PP) |
COPYLENE®
|
| Phillips 66 COPYLENE® CM015G Polypropylene Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM360N Polypropylene, Impact Copolymer, Injection Molding |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CR300CL-01 Polypropylene Random Copolymer |
Polypropylene Copolymer |
COPYLENE®
|
| Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer |
Polypropylene Copolymer |
COPYLENE®
|