Material Notes:
3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Tape
76.2 microns
3.00 mil
Release Liner
Mechanical Properties Metric English Comments
Peel Strength 0.49303 kN/m
2.8125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Short term
177 °C
351 °F
Long term
Descriptive Properties Value Comments
Adhesive Type 430
Appearance Clear
Liner Tan 60# Densified Kraft