Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FT 2481 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Dyneon™ Fluoroelastomer FT 2481 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FT 2481 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Composition: Terpolymer of vinylidene fluoride, hexafluoropropylene, and tetrafluoroethyleneTerpolymer gumstock without incorporated curativesProcess targets: compression moldingImproved retention of elongation after long term heat aging compared to conventional 66% fluoropolymerImproved acid resistance and improved resistance to volume swell by organic solvents compared to conventional 66% fluoropolymersFT 2481 is amine or bisphenol curableInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.86 g/cc
1.86 g/cc
Mooney Viscosity 75

@Temperature 121 °C
75

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 220 %
220 %
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00551 GPa
0.799 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 24 %
24 %
Aged 70 hours @ 200°C, -214 O-rings; ASTM D395 Method B
Thermal Properties Metric English Comments
Transformation Temperature -14.0 °C
6.80 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 68.6 %
68.6 %
Descriptive Properties Value Comments
Color Translucent Amber
MH, Maximum Torque 20.6 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 2.7 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Ketones and Esters
t`50, Time to 50% cure 4.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure @ 177°C - minutes 5.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min @ 177°C - min 3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C