Arlon LW201C##FR-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arlon LW201C##FR-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: High Strength, 1 inch wide, 20 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length in yards.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone RubberCross-Section: 1” Wide TriangularFAR 25.853 Recognition: Product is designed to meet the FAR 25.853 App.F, P.1,.Aii flame resistance requirements but is not recognized by an FAA test Laboratory.UL Recognition The product is designed to meet UL94V-0 flame resistance requirements but is not recognized by Underwriters Laboratories. Arlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent wraps in order to form a uniformly thick layer.Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wrapped around complex forms.Bonds to itself at room temperature within 24 hours.Remains non-tacky to the touch and does not adhere to other surfaces, or substrates.Insulates with single wrap, thereby reducing labor time and cost.Dampens vibration and resists heat and mechanical shock as well as corona.Inherently flame resistant and when burned forms a non-conductive ash.SA & SB MOX-Tapes® provide a uniform thickness even around sharp edges. Fiberglass fabric, encapsulated inside the silicone rubber, prevents wicking and maintains high insulation resistance under high humidity conditions. These controlled stretch tapes provide a uniform insulation barrier.All tapes are protected by a special interleaved liner.Applications:Mechanical:Protection of coils from vibration.Vibration fixture, anti-scratch, and clamping pads.Harness wrapping and wire bundling, including for high temperature applications.Applied to rollers for protection and traction.Plant maintenance.Superior, heavy duty repair tape for emergency insulating barrier.Electrical:Insulation of field armature and interpole coils in large motors.Insulation for splicing and terminating of wire and cable.Insulating and sealing electrical connections.Insulating coil leads and bus bar connections.Electromagnetic coil insulation.Motor connections.Overwrapping of deteriorated insulation in reclaimed motors.Environmental:On-board aviation and space applications.Underground cable splices.Insulating heated transfer lines.Insulating in radioactive environments.Masking agent utilized in manufacturing processes and powder coatings.Insulating, protecting, and sealing rigging hardware and power systems in marine applications.This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.0 %
1.0 %
Arlon SQA-TMS-016
Thickness 76.2 microns
3.00 mil
Interleave
508 microns
20.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 6.87 MPa
997 psi
Silicone Property; ASTM D412
Elongation at Break 477 %
477 %
Silicone Property; ASTM D412
Peel Strength 0.473 kN/m
2.70 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Flammability, UL94 V-0
V-0
Flammability Test 0.70
0.70
[in], Char Length; FAR 25.853 App. F, P.1,.Aii
3.3
3.3
[sec], Flame and Glow; FAR 25.853 App. F, P.1,.Aii
Electrical Properties Metric English Comments
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Brown