Material Notes:
3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and application consideration. Due to poor flow properties of the micropowder it is recommended that the micropowder and matrix material both be at a temperature below 30°C (86°F). However, in the case of thermoplastic blends, the micropowder may be incorporated into the melt. Dyneon PTFE Micropowder J14 can be dispersed using a variety of mixing equipment. Depending upon the application, high speed mixers and tumble blenders have been successful for dry blends, while propeller mixers work well for wet mixtures such as solvents and oils. Glass bead mills should be used for relatively high viscosity mixtures and roll mills for very high viscosity applications, such as lubricating greases and oils.Low molecular weight PTFE powderAgglomerate particlesFriableHigh specific surface areaBroad chemical resistance and temperature range of useInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.250 g/cc
0.00903 lb/in³
ASTM D4895
Particle Size 2.0 µm
2.0 µm
Hegman; Grinde Gauge
6.0 µm
6.0 µm
Laser Diffraction