3M Dyneon™ PVDF 1012/0001 Polyvinylidene Fluoride  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Dyneon™ PVDF 1012/0001 Polyvinylidene Fluoride  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High molecular weight grade PVDFSuitable for compression molding or extrusionExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Water Absorption <= 0.040 %
<= 0.040 %
24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound 0.50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
0.50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
1.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 230 °C
1.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 446 °F
ASTM D1238
5.0 g/10 min
<br>@Load 10.0 kg,<br> Temperature 230 °C
5.0 g/10 min
<br>@Load 22.0 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
Tensile Strength, Yield 55.0 MPa
7980 psi
50mm/min; ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
50mm/min; ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
2mm/min; ASTM D790
Thermal Properties Metric English Comments
Melting Point 174 °C
345 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
Flammability, UL94 V-0
V-0
Oxygen Index >= 44 %
<br>@Thickness 3.00 mm
>= 44 %
<br>@Thickness 0.118 in
Sheet; ASTM D2863
Descriptive Properties Value Comments
Form Pellets