Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ TF 2029 PTFE  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 2029 PTFE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Processable by standard paste extrusion methodsDesigned for low reduction ratiosCan be processed at a high stretch ratiosRecommended for apes requiring high mechanical strength, such as electrical tape for wrapped insulation or flat cablesRecommended for yarn applications, such as sewing or weaving yard for filter and sealing materials or dental flossCan be used to extrude pipe liners requiring green strength higher that TF 2025Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.480 g/cc
0.0173 lb/in³
ISO 12086
Density 2.15 g/cc
0.0777 lb/in³
ISO 12086
Particle Size 500 µm
500 µm
average; ISO 12086
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ISO 12086
Elongation at Break 340 %
340 %
ISO 12086
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+19 ohm-cm
1.00e+19 ohm-cm
IEC 60093
Surface Resistance 1.00e+18 ohm
1.00e+18 ohm
IEC 60093
Descriptive Properties Value Comments
Extrusion Pressure 50 MPa
reduction ratio 400, ASTM D4894
Reduction Ratio Range 5-100:1
Dyneon Method