3M Dyneon™ TF 2072Z PTFE Fine Powder

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 2072Z PTFE Fine Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dyneon™ TF 2072 Z PTFE is an ideal grade for thin-wall, small diameter tubing and wire and cable insulations, processed by paste extrusion method at reduction ratio up to 3000:1. This product offers more economic processing because of larger usable preforms.Product Features:High molecular weightNeeds less lubricant than TF 2071 Z (1-2 parts by weight)Emulsion polymerization PTFE Product grade with lower extrusion pressure than TF 2071 ZMeets ASTM D4895-04 Type 1, Grade 1, Class C classificationProcessing by standard paste extrusion methods Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.470 g/cc
0.0170 lb/in³
DIN EN ISO 60
Density 2.17 g/cc
0.0784 lb/in³
DIN EN ISO 12086
Particle Size 440 µm
440 µm
average; ISO 13320
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
DIN EN ISO 527-3
Elongation at Break 470 %
470 %
DIN EN ISO 527-3
Descriptive Properties Value Comments
Extrusion Pressure 40 MPa
reduction ratio 400:1, ASTM D4895
Reduction Ratio Range 50-3000:1
Dyneon Method