Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ THV 500GZ Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ THV 500GZ Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
THV 500G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature processing, low flammability, thermal stability, and melt processability. It can be used to prepare molded parts and extruded films, tubes, profiles and wire coatings. It is useful for applications that require flexibility, low temperature processing and good chemical resistance.Features and Benefits: Excellent flexibilityProcessing profile allows coprocessing with olefinic plastics and hydrocarbon elastomers Excellent chemical and permeation resistanceHigh transparencyLow flammabilityBondable to itself and other substrates (for multi-layer constructions)Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D792
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 265 °C
10 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D4591
Oxygen Index >= 75 %
>= 75 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Form Pellets
Users viewing this material also viewed the following: