3M FM1732R White Polyester Label Products

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FM1732R White Polyester Label Products.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ White Polyester Label Products FM1732 and FM1732R are durable, high performance materials that offer excellent thermal stability. These polyester label products utilize 3M™ Adhesive R3500, which is designed for use on smooth surfaces such as glass, metal and plastic (including polystyrene) and offers excellent UV resistance, good initial tack, and long term adhesion with clean removability and is an excellent alternative to static cling.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Facestock
78.7 microns
3.10 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.0526 kN/m
0.300 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 43.0 °C
109 °F
Application
68.0 °C
154 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type R3500 Rem 16
Liner 50# SC Remoist