3M Scotch-Weld™ DP608 Structural Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP608 Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible and Non-sagInformation provided by 3M
Mechanical Properties Metric English Comments
Shear Strength 13.8 MPa
2000 psi
Processing Properties Metric English Comments
Cure Time 90.0 min
1.50 hour
Time to Handling Strength