5370 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 5370 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D412
Tensile Strength, Yield 31.0 MPa
4500 psi
at 100%; ASTM D412
Elongation at Break 180 %
180 %
ASTM D412
Tear Strength 158 kN/m
900 pli
die B; ASTM D624