A. Schulman POLYBATCH™ Buff 60234 Concentrate Based In LDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Buff 60234 Concentrate Based In LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPOLYBATCH® 60234 is a buff color concentrate based in LDPE. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 60234 is heavy metal free and is typically recommended for use at 5% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.72 g/cc
1.72 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 61 %
61 %
Descriptive Properties Value Comments
Moisture (max) 1500
ppm, ASTM D789
Pellet Count 55
pellets/gram