Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc

@Temperature 20.0 °C
0.284 lb/in³

@Temperature 68.0 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 340 MPa
>= 49300 psi
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
Elongation at Break >= 25 %
>= 25 %
Modulus of Elasticity 200 GPa

@Temperature 20.0 °C
29000 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 20.0 - 100 °C
6.89 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
Users viewing this material also viewed the following: