Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS)

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Typical Carbon Steel
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 380 MPa
>= 55100 psi
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
Elongation at Break >= 16 %
>= 16 %
Modulus of Elasticity 201 GPa
29200 ksi
88.3 GPa

@Temperature 649 °C
12800 ksi

@Temperature 1200 °F
183 GPa

@Temperature 316 °C
26500 ksi

@Temperature 600 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F