Abatron AboCast 8-3/Abocure 8-3 Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-3/Abocure 8-3 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.22 %
0.22 %
in 24 hours.
Viscosity Measurement 1600
1600
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Tensile Strength, Ultimate 58.61 MPa
8501 psi
Elongation at Break 5.5 %
5.5 %
Flexural Strength 94.8 MPa
13700 psi
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.0 °C
163 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 4.80e+11 ohm-cm

@Temperature 93.3 °C
4.80e+11 ohm-cm

@Temperature 200 °F
6.20e+14 ohm-cm

@Temperature 65.6 °C
6.20e+14 ohm-cm

@Temperature 150 °F
3.60e+15 ohm-cm

@Temperature 25.0 °C
3.60e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.33

@Frequency 1e+6 Hz
3.33

@Frequency 1e+6 Hz
Dissipation Factor 0.017

@Frequency 1e+6 Hz
0.017

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 16 hours; Postcure: 2 hours/100°C (212°F)