Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
MD; ASTM D955
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 53
53
ASTM D785
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM D638
Flexural Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 2.499 GPa
362.5 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F