| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 3.28 - 3.31 g/cc | 3.28 - 3.31 g/cc | ASTM D792 |
| Deformation | 7.0 - 10 % | 7.0 - 10 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 56 - 58 | 56 - 58 | ASTM D2240 |
| Ball Indentation Hardness | 46.0 - 50.0 MPa | 6670 - 7250 psi | ISO 2032-N132 |
| Tensile Strength at Break | >= 20.0 MPa | >= 2900 psi | ASTM D4745-11 |
| Elongation at Break | >= 220 % | >= 220 % | ASTM D4745-11 |
| Coefficient of Friction, Dynamic | 0.13 - 0.15 | 0.13 - 0.15 | ASTM D1894 |
| Coefficient of Friction, Static | 0.15 - 0.16 | 0.15 - 0.16 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
| Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |