| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Adalon® 817 PTFE, 60% Bronze.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 3.88 - 3.90 g/cc | 3.88 - 3.90 g/cc | ASTM D792 |
| Deformation | 4.0 - 6.0 % | 4.0 - 6.0 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 60 - 64 | 60 - 64 | ASTM D2240 |
| Ball Indentation Hardness | 57.0 - 60.0 MPa | 8270 - 8700 psi | ISO 2032-N132 |
| Tensile Strength at Break | >= 16.0 MPa | >= 2320 psi | ASTM D4745-11 |
| Elongation at Break | >= 160 % | >= 160 % | ASTM D4745-11 |
| Coefficient of Friction, Dynamic | 0.16 - 0.18 | 0.16 - 0.18 | ASTM D1894 |
| Coefficient of Friction, Static | 0.18 - 0.20 | 0.18 - 0.20 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
| Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |