Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adamas Hardor® 991 PE-UHMW

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Adamas
Trade Name Hardor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Hardor® 991 PE-UHMW.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 0.920 - 0.930 g/cc
0.920 - 0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 58 - 60
58 - 60
ASTM D2240
Ball Indentation Hardness 34.0 - 36.0 MPa
4930 - 5220 psi
ISO 2039-1
Tensile Strength at Break >= 40.0 MPa
>= 5800 psi
ASTM D4894
Elongation at Break >= 350 %
>= 350 %
ASTM D4894
Thermal Properties Metric English Comments
Thermal Conductivity 0.410 W/m-K
2.85 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 193 °C
379 °F
DSC
Maximum Service Temperature, Air 110 °C
230 °F
DSC
Minimum Service Temperature, Air -180 °C
-292 °F
DSC
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
ASTM D257
Dielectric Strength 45.0 kV/mm
1140 kV/in
ASTM D149